"step_id": "research",
"agent": "webster",
"status": "complete",
"result": "The Young's modulus for Invar 36 is typically around 141 GPa (20.5 x 10^6 psi) for annealed material. For cold-rolled strip, it can be slightly higher, around 148 GPa (21.5 x 10^6 psi).",
"notes": "The value can vary slightly depending on the material's condition (e.g., annealed vs. cold-rolled). Source: High Temp Metals technical data sheet.",
"run": {
"schemaVersion": "1.0",
"runId": "orch-1771180163-569e1d0d",
"agent": "webster",
"status": "complete",
"result": "The Young's modulus for Invar 36 is typically around 141 GPa (20.5 x 10^6 psi) for annealed material. For cold-rolled strip, it can be slightly higher, around 148 GPa (21.5 x 10^6 psi).",
"artifacts": [],
"confidence": "high",
"notes": "The value can vary slightly depending on the material's condition (e.g., annealed vs. cold-rolled). Source: High Temp Metals technical data sheet.",
"timestamp": "2026-02-15T18:29:46Z",
"latencyMs": 27786,
"workflowRunId": "wf-1771180163-49f868ac",
"stepId": "research",
"exitCode": 0
},
"started_at": "2026-02-15T18:29:23.361620+00:00",
"finished_at": "2026-02-15T18:29:51.273466+00:00",
"duration_s": 27.912
}